  • Article Code : FIRAT-AKADEMI-8211-4211
  • Article Type : Araştırma Makalesi
  • Publication Number : 2A0146
  • Page Number : 165-171
  • Doi : 10.12739/NWSA.2018.13.2.2A0146
  • Abstract Reading : 548
  • Download : 138
  • Share :

  • PDF Download

Issue Details

  • Year : 2018
  • Volume : 13
  • Issue : 2
  • Number of Articles Published : 14
  • Published Date : 1.04.2018

Cover Download Context Page Download
Technological Applied Sciences

Serial Number : 2A
ISSN No. : 1308-7223
Release Interval (in a Year) : 4 Issues

MEKANİK ALAŞIMLAMA/ÖĞÜTME YÖNTEMİ İLE ÜRETİLEN Al-SiC KOMPOZİTLERİN İNCELENMESİ

İjlal ŞİMŞEK1 , MUSA YILDIRIM2 , Tansel TUNÇAY3 , Dursun ÖZYÜREK4 , Doğan ŞİMŞEK5

Bu çalışmada, mekanik öğütme yöntemiyle üretilen Al-bazlı kompozit malzemelerin üretiminde farklı miktarlarda ilave edilen SiC ve öğütme süresinin mikroyapı, yoğunluk ve sertlik üzerine etkisi incelenmiştir. Çalışma kapsamında, alüminyum matrise farklı miktarlarda (%5, %10, %15 ve %20) SiC ilave edilerek 4 farklı sürede (30, 60, 90, 120 dakika) mekanik öğütülmüştür. Atritör tipi mekanik alaşımlama cihazında öğütme elemanı olarak 6mm çapında çelik bilya, 750 devir/dakila’lık öğütme hızı, 10:1 bilya-toz oranı, işlem kontrol kimyasalı olarak %2 stearik asit kullanılmıştır. Kompozit tozların üretimi argon ortamında yapılmıştır. Üretilen kompozit tozlar tarama elektron mikroskobu, EDS analizleri, optik mikroskop ve toz boyut analizörü kullanılarak karakterize edilmiştir. Yapılan çalışmalar sonucunda, ilave edilen SiC miktarı ve öğütme süresi arttıkça toz boyutunda azalma görülürken, sertlik değerlerinde artış görülmektedir. Bununla birlikte ilave edilen SiC miktarı arttıkça da yoğunlukta artış görülmektedir.

Keywords
Alüminyum Kompozit, Mekanik Öğütme, Toz Metalürjisi, Atritör, SiC,

AN INVESTIGATION OF Al-SiC COMPOSITES PRODUCED BY MECHANICAL ALLOYING/MECHANICAL MILLING METHOD

İjlal ŞİMŞEK1 , MUSA YILDIRIM2 , Tansel TUNÇAY3 , Dursun ÖZYÜREK4 , Doğan ŞİMŞEK5

In this study, the effects of different amount of SiC content and different milling time on the microstructure, density and hardness of Al based composites were investigated. In the scope of the study, four different amount of SiC (5%, 10%, 15%, 20%) were added into Al and mechanical milled four different time (30 min, 60 min, 90 min, 120 min). In the mechanical milling procedure, attritor type milling device was used for 750 rpm milling speed with 2% stearic acid as a process control chemical under argon atmosphere, stainless steel balls of a dimension of 6mm, ball/powder ratio of 10:1 were used. Produced powder composites were characterized by scanning electron microscope, EDS, powder size analyzer. As a result of the study, powder size was decreased and also increased hardness values with increasing amount of SiC content and milling time. In addition, density values were increased by increasing amount of SiC content.

Keywords
Aluminum Composite, Mechanical Milling, Powder Metallurgy,, Attritor, SiC,

Details
   

Authors

İjlal ŞİMŞEK (1) (Corresponding Author)

Milli Savunma Üniversitesi
isimsek@msu.edu.tr | 0000-0001-6542-8567

MUSA YILDIRIM (2)

musayildirim@karabuk.edu.tr | 0000-0002-7762-8504

Tansel TUNÇAY (3)

Karabük Üniversitesi
tanseltuncay@karabuk.edu.tr | 0000-0002-7762-8504

Dursun ÖZYÜREK (4)

dozyurek@karabuk.edu.tr | 0000-0002-8326-9982

Doğan ŞİMŞEK (5)

dsimsek@beu.edu.tr | 0000-0001-8339-9704

Supporting Institution

:

Project Number

:

Thanks

:
References
[1] Benjamin, J.S., (1976). Mechanical Alloying, Scientific American, Volume:234, Number:5, pp:40-48.