• icon+90(533) 652 66 86
  • iconnwsa.akademi@hotmail.com
  • icon Fırat Akademi Samsun-Türkiye

Article Details

  • Article Code : NWSA-2359-1403
  • Article Type : Araştırma Makalesi
  • Publication Number : 1A0093
  • Page Number : 416-427
  • Doi : 10.12739/
  • Abstract Reading : 1299
  • Download : 157
  • Share :

  • PDF Download

Issue Details

  • Year : 2010
  • Volume : 5
  • Issue : 2
  • Number of Articles Published : 14
  • Published Date : 1.04.2010

Cover Download Context Page Download
Ecological Life Sciences

Serial Number : 5A
ISSN No. : 1308-7258
Release Interval (in a Year) : 4 Issues

KAĞIT ENDÜSTRİSİNDE BENTONİT İLE BİRLİKTE KULLANILAN POLİMERLERİN TUTUNMA VE KAĞIT ÖZELLİKLERİ ÜZERİNE ETKİSİ

Ahmet TUTUS 1

Bu çalışmada, ağartılmış sülfat kağıt hamurları kullanılmış ve bentonit ile birlikte kullanılan polimerlerin tutunma ve kağıt özellikleri üzerine etkisi araştırılmıştır. Tutunma, kağıdın yüzey düzgünlüğü, fiziksel ve optik özelliklerini, kağıt maliyetini ve atık su arıtma tesislerinin yükünü etkilemektedir. Kırıntı lif kaybını minimuma indirmek için bentonit ile birlikte anyonik ve katyonik polimerleri (percol 156, percol 3030, basf luredur, poli-dadmac ve kartaretin) kullanılmıştır. %0.2 oranında bentonit ve %0.2 polimer kullanımında maksimum tutunma olduğu bu oranın yükseltilmesi durumunda tutunma oranın azaldığı tespit edilmiştir. Bentonit ile birlikte kullanılan polimerler genel olarak kağıdın fiziksel direnç özelliklerini artırmış, optik özelliklerini ise azaltmıştır.

Keywords
Tutunma, Bentonit, Polimer, Kağıt, Fiziksel ve Optik Özellikler,

THE EFFECT OF POLYMERS USED WITH BENTONITE IN PAPER INDUSTRY ON RETENTION AND PAPER PROPERTIES

Ahmet TUTUS 1

In this study, bleached sulfate pulps used as raw material and the effects of polymers used with bentonite in paper industry on retention and paper properties were investigated. Retention has influence on paper properties like smoothness, physical and optical properties, on the cost of paper produced and the mill effluent treatment. For minimized to fine loss anionic and cationic polymer (percol 156, percol 3030, basf luredur, poli-datmac and cartaretin) with bentonite were used. The maximum retention was detrmined in usage 0.2% bentonite and 0.2% polymer. Since bentonite and polymer values added above 0.2% in furnish retention were decreased. In general, polymers used with bentonite were increased the strength and decreased the optical properties.

Keywords
Retention, Bentonite, Polymer, Paper, Physical and Optical Properties,